← Frame making

Heated die

A long heated die where the resin sets and the pultruded profile takes its shape.

The resin-soaked fibers are pulled into the die, about a meter long with several heating zones at up to 230 °C. By the time they leave it the resin has set hard. The die temperature and length are matched to the resin and the line speed, which is typically up to 2 or 3 meters a minute.

After the puller, the profile is cut to length with a saw.

A fiberglass line in elevation, from the glass furnace and bushing to the pultrusion line

Hover or tap a part to see what it is called.

Fiberglass line, from glass furnace to pultruded profile, in elevation

Related