Surface compression
The squeeze locked into the faces of tempered glass, which makes it strong.
Glass breaks from cracks at its surface pulled open by tension. The quench cools the faces first, and as the core cools and shrinks it pulls them into compression. A crack has to overcome that compression before it can open. Fully tempered glass has at least 10,000 psi of surface compression and heat-strengthened glass 3,500 to 7,500 psi.