← Glass types

Heat soak test

Also called HST, heat soaking

Baking tempered glass at about 290 °C so panes with dangerous inclusions break in the factory.

After tempering, panes are held in an oven at around 290 °C. The heat speeds up the change in any nickel sulphide inclusions, so panes that would have broken in the building break in the oven instead. It catches about 95% of them, and it is required for some facade uses.